RBCuZn-C

  • AWS A5.8:      RBCuZn-C

Chemical Composition: %

CuSnSiFeMnZnOther
56-600.8-1.10.04-0.150.25-1.200.01-0.5Balance0.5

joining process

  • Acetylene torch, induction and resistance heating

Description and Applicaiton

  • Brazing alloy with good flowing properties, hardly sensitive to overheating.
    Suitable for gap brazing and coating of steel, cast iron, malleable cast iron,
    as well as copper and copper alloys with a solidus of > 900 °C.

Availability

  • Rods: φ1.5-5.0mm  Length: 1000mm

    Wire:  φ0.8, 1.0, 1.2, 1.6mm on spools D300

    Other dimensions are available upon request

Mechanical and physical properties

  • Working temperature: 910-955 °C
    Melting range: 866-888 °C
    Density: 8.4 g/cm³