ERNiCrFe-6

  • AWS A5.14:    ERNiCrFe-6  

    EN ISO 18274: SNi 7092   

Chemical Composition: %

CNiFeTiCSiMnPCuOther
14-17≥67≤8.02.5-3.5≤0.08≤0.352.0-2.7≤0.0150.50.50

Mechanical and physical properties

  • Tensile strength: 553 Mpa

    Yield Strength:  248 MPa
    Elongation: 31 %

    Brinell Hardness: 132 HBW

Welding process

  • TIG , MIG

Description and Applications

  • Solid wire for dissimilar joints. Use for Mig and Tig welding of dissimilar alloys: Nickel alloys to stainless steels, carbon steels, and Nickel-copper alloys (e.g. Monel®); Nickel-copper alloys and pure Nickel to stainless steels; stainless steels to carbon steels.

    This wire provides high strength and corrosion resistance from -269°C to over 980°C. Weld deposits can be age hardened for greater strength at temperatures to about 700°C

Availability

  • Rods: φ1.5-5.0mm  Max.Length: 1000mm

    Wire:  φ0.8,1.0,1.2,1.6mm on spools D300

    Other dimensions are available upon request

BEIDUO Alloys Newsletter

Sign up for our Newsletter and receive updates on events, collections and exclusive promotions.

I have read the Privacy Policy

CUSTOMER CARE

PROCDUCTS

CONTACT US

FOLLOW OUR COMMUNITY SOCIAL MEDIA